RTP Co., Winona, Minn., has come out with a series of biocompatible styrenic-based TPEs for use in medical devices.
RTP Co., Winona, Minn., has come out with a series of biocompatible styrenic-based TPEs for use in medical devices. The RTP 2700 S MD Series (30 to 80 Shore A) has been pretested for ISO 10993-5/10/11 biocompatibility standards and offers gamma-radiation and ethylene oxide (EtO) sterilizability. They bond well to PP in overmolding. They are also cost-competitive with medical-grade TPVs and TPOs. They are clear with a neutral color suitable for use in many Class I and Class II devices.