WEB EXCLUSIVE: Surpass IGs153-A resin is a new octene-copolymer HDPE for injection and compression molding water-bottle caps.
WEB EXCLUSIVE: Surpass IGs153-A resin is a new octene-copolymer HDPE for injection and compression molding water-bottle caps. Supplied by Nova Chemicals Corp., Moon Township, Pa., It reportedly offers superior organoleptic properties that allow it to pass tests for one-piece, linerless closures by several major global water bottlers. This resin also performs well in the newer short-height bottle finishes. The resin has a density of 0.953 g/cc and melt index of 1.5 g/10 min.