WEB EXCLUSIVE: Three new series of polyesters are newly offered by compounder and distributor KMI Group, Newport Beach, Calif., through an exclusive distribution agreement with an unnamed supplier.
WEB EXCLUSIVE: Three new series of polyesters are newly offered by compounder and distributor KMI Group, Newport Beach, Calif., through an exclusive distribution agreement with an unnamed supplier. The PBT series consists of 10-40% glass-filled grades in black and natural color. Also available in both black and natural are biodegradable PBAT (polybutylene adipate co-terephthalate) and PBSA (polybutylene succinate adipate) resins. The degradable materials are offered in both a low-melt-flow version for sheet extrusion and a high-flow version for injection molding.