WEB EXCLUSIVE: Solvay Advanced Polymers, LLC, Alpharetta, Ga., is supplying its KetaSpire PEEK to Entegris Inc., Billerica, Mass., which formulates Tego compounds using carbon nanotubes. Entegris uses proprietary compounding technology to achieve uniform dispersion of nanotubes in order to provide uniform electrical and thermal conductivity throughout molded or extruded parts. Tego PEEK/nanotube compounds are aimed at medical, aerospace, automotive, and oil/gas applications requiring electrostatic dissipation and/or thermal management. While Entegris produces pellets, its PEEK/nanotube products are also available in extruded rod and plate stock shapes from Quantum Polymers, Newark, Del.