MATERIALS: Polyketone Compounds Are Back

Discontinued engineering polymer reappears after 14 years.

Lehvoss North America, Pawcatuck, Conn., is introducing Luvocom 70 series engineering compounds based on polyketone (PK) resin. These compounds are said to fill a gap separating nylon 6 and 66 and acetal from resins like PPS, PEI and PAEK. “The introduction is actually a re-launch,” says Michael Sandeen, sales and business development manager. “Luvocom 70 products had been available until the year 2000 but had to be canceled due to Shell Chemical’s discontinuation of Carilon PK polymer production.” With the polymer now available (produced by at least three companies in China and Korea), Lehvoss resumed development of these high-performance compounds.
 
PK reportedly offers good hydrolytic stability, low water absorption, low permeability, good weld-line strength, and good processability, with shorter cycle times than nylon 66 and acetal. “In many cases, PK is better than acetal and nylons,” says Sandeen. “It can replace even high-temperature polymers in tribological applications. Its low wear rate offers excellent advantages for gear wheels and bearings.” And its high chemical resistance is said to suit PK to fuel filters and other fuel-system components.
 
Luvocom 70 currently comes in three grades: 70-9045 reinforced with carbon fibers; 70-9046 lubricated with PTFE; and 70-9113/BK formulated for low friction and wear.