MATERIALS: Purging Agent in New Packaging for Medical Clean Rooms

A new packaging option for Ultra Purge purging agent was developed specifically for clean-room production of medical parts.

Related Topics:

Related Suppliers

A new packaging option for Ultra Purge purging agent, developed specifically for clean-room production of medical parts, is available from Moulds Plus International USA, Santa Ana, Calif. Previously, Ultra Purge was only offered in cardboard packaging, which in certain situations is not allowed in clean rooms. The new 5-lb packaging option is an HDPE bottle with a screw-on PE cap.