WEB EXCLUSIVE: Solvay Specialty Polymers has unveiled a range of recycled grades of Solef PVDF.

Related Suppliers

WEB EXCLUSIVE: Solvay Specialty Polymers (U.S. office in Alpharetta, Ga.) has unveiled a range of recycled grades of Solef PVDF. Called Fluorloop, the new series is based on recycled scrap from the Solef production process as well as post-molding scrap from Solvay customers. It was developed through a global partnership with Paris-based Agiplast, a compounder and recycler of engineering resins. A range of Fluorloop grades are available for extrusion, injection, and compression molding.