MATERIALS: Tougher Long-Fiber Nylon Compounds

WEB EXCLUSIVE: New nylon 6 and 66 compounds with up to 60% long-glass fiber are said to be “ultra-durable,” with up to twice the impact resistance of standard materials.

Related Suppliers

WEB EXCLUSIVE: New nylon 6 and 66 compounds with up to 60% long-glass fiber are said to be “ultra-durable,” with up to twice the impact resistance of standard materials. New Complet MT (maximum toughness) pellets from PlastiComp, Inc., Winona, Minn., boast outstanding injection moldability suitable for complex shapes and thin walls. They are also colorable for applications in sporting goods, consumer durables, and large appliances.