Evonik Cyro LLC (formerly Cyro Industries), Parsippany, N.J., has introduced two Acrylite MD grades of PMMA acrylic molding resins for medical uses. Both grades meet FDA 21CFR177.1010 specs and are suitable for USP Class VI uses in containers and diagnostic accessories, such as cuvettes, test packs and rotors, and crystallography trays. Acrylite MD is produced with strict quality control for UV transmittance (87.7% transmittance at 340 nm), essential for consistent measurement response. The two grades are Acrylite MD L40 with 26 MFR and grade MD H12 with 7 MFR. For complete property details, visit www.ptonline.com/plaspec. (800) 631-5384 • www.cyro.com