A new acetal from DuPont Engineering Polymers, Wilmington, Del., is formulated with a proprietary metallic filler for molding chain-link food-processing conveyors. The filler in Delrin 400MTD can be detected by most metal-sensing equipment in the unlikely event that part of the conveyor enters the process stream. The new acetal has high strength and stiffness with minimal effect on impact and elongation. It complies with FDA Regulation 21-CFR177.2470 for food contact on a repeated-use basis. Tel: (800) 4410575 • www.plastics.dupont.com