WEB EXCLUSIVE: The award-winning Ford Fusion Hybrid car has an “eco-friendly” engine cover with a molded-in metallic look instead of paint.
WEB EXCLUSIVE: The award-winning Ford Fusion Hybrid car has an “eco-friendly” engine cover with a molded-in metallic look instead of paint. It thereby eliminates the extra energy expenditure and VOC emissions associated with painting. The cover was created by MPC Inc., Walworth, Wis., using Maxxam FX Metal talc-filled PP compound from PolyOne Corp., Cleveland. (866) 765-9663 • polyone.com
PolyOne Corp.
33587 Walker Rd. Avon Lake, OH 44012
Phone (440) 930-1000 Fax (216) 589-4077