A new mold release is designed for urethane elastomers used in auto interiors.
A new mold release is designed for urethane elastomers used in auto interiors. Mold Release Coating 7642 from Huron Technologies, Inc., Leslie, Mich., is designed to minimize build-up on the mold surface and increase the time between mold cleanings. It is also said to maintain low gloss and consistent surface appearance and release for all areas of large, complex molds. (517) 589-3000 • www.hurontech.com
Huron Technologies
415 Industrial Dr. Leslie, MI 49251