Molder & Moldmaker Embraces Minimalist Tooling Philosophy
RenyMed’s niche consists of projects where it can offer not only molding, but help in designing and making the unique, compact, modular tools that are a company specialty.
RenyMed CEO Steve Raiken half-jokingly calls it his “Harry Potter closet.” The walls of the 6 x 8 ft space off the tool room are lined with shelves filled with small plastic containers. They give the initial impression that this is a compact storage area for various mold components. On closer inspection, however, visitors discover that each blue plastic container holds a production tool slid into protective netting.
For most injection molders, tool storage consists of pallet-lined floor-to-ceiling racks, where molds are moved to and from production by a combination of forklifts and overhead cranes. However, RenyMed, Baldwin Park, Calif., can store all its tooling in what amounts to a closet, with workers pulling a mold from its netting and dropping it into the appropriate modular base, which RenyMed also makes.
Says Raiken, “When we tell a potential customer we have a unique modular system, almost always they ask, ‘Is it a M.U.D. base?’ We show them 4-in. round cavity mold insert set with a robust 1/2-in. cooling channel that envelops the cavity, double slides that inter- lock the cavity, a side Y-corepull, and a helical unwind for a luer thread.
“We then install all this in a mold base with guided ejection and it becomes an SPI class 101 mold without an ejector pin mark on the part. The customer then says they have never seen a solution such as this. We then tell them this is scalable to four cavities. This is unique.” This modular tooling concept was developed by RenyMed about seven years ago. While it’s not a fit for every project, in the programs where it does work, it offers myriad benefits. In addition to shorter lead times, the compact tools require minimal storage space and can run on smaller machines. Those floorspace-saving benefits add up quickly in the costly California real-estate market.
From a production standpoint, the compact tooling minimizes residence time for the expensive, heat-sensitive resins RenyMed uses to mold precision medical components.
“Because it’s modular, we’re starting from the 40-yard line in terms of design,” says Raiken. “We’re getting a running start on the project.” As an example, he displays one part for which RenyMed was able to create tools for six different sizes in seven weeks.
“We make the most contained and concise mold,” Raiken says. “So, when we use this tooling, what we’re doing is asking, ‘What does the part require?’ rather than fitting the part into something we know.”
Raiken knows molds, having started a one-man tool shop in the mid-1980s after completing a moldmaking apprenticeship. That operation was carved out of unused space in the corner of an injection molder, and consisted of a mill, grinder, and lathe. Dissatisfied with the mold testing he was finding, Raiken decided to add a molding machine, which he did in a new space all to himself.
Raiken expanded his business from there, taking on molding and growing along with the California medical-device market, which called for high-precision parts made from difficult materials in a race to the smallest that continues today. Ten years ago, RenyMed moved into its current space in Baldwin Park.
Raiken notes that most of the parts he makes weigh less than a gram. Exemplifying the small size and precise nature of the programs RenyMed takes on, when Plastics Technology visited, Raiken was preparing for a customer visit to discuss a new ophthalmology product used to hold the iris open during cataract surgery. For this project, as with well over 90% of its jobs, RenyMed will help design the tooling it will build and run.
“Our niche is creative DFM [design for manufacturing]. We provide our customers with creative manufacturing solutions that help them realize their medical device,” Raiken says. “At trade shows, molders lay out hundreds of parts, to say, ‘That’s what we do, we make plastic parts.’ Well that’s not what we do. We provide our customers with the ability to make their product.”
Related Content
Why Shoulder Bolts Are Too Important to Ignore (Part 1)
These humble but essential fasteners used in injection molds are known by various names and used for a number of purposes.
Read MoreImprove The Cooling Performance Of Your Molds
Need to figure out your mold-cooling energy requirements for the various polymers you run? What about sizing cooling circuits so they provide adequate cooling capacity? Learn the tricks of the trade here.
Read MoreBest Methods of Molding Undercuts
Producing plastics parts with undercuts presents distinct challenges for molders.
Read MoreWhat You Need to Know About Leader Pins and Bushings
There’s a lot more to these humble but essential mold components than you might suspect. Following the author’s tips could save much time, money and frustration.
Read MoreRead Next
Advanced Recycling: Beyond Pyrolysis
Consumer-product brand owners increasingly see advanced chemical recycling as a necessary complement to mechanical recycling if they are to meet ambitious goals for a circular economy in the next decade. Dozens of technology providers are developing new technologies to overcome the limitations of existing pyrolysis methods and to commercialize various alternative approaches to chemical recycling of plastics.
Read MoreUnderstanding Melting in Single-Screw Extruders
You can better visualize the melting process by “flipping” the observation point so that the barrel appears to be turning clockwise around a stationary screw.
Read More