WEB EXCLUSIVE: In November, we incorrectly reported that Mold-Masters Ltd., Georgetown, Ont., had introduced at the NPE show complete hot halves for PET preforms with up to six drops.
WEB EXCLUSIVE: In November, we incorrectly reported that Mold-Masters Ltd., Georgetown, Ont., had introduced at the NPE show complete hot halves for PET preforms with up to six drops. In fact, Mold-Masters has teamed up with ABBA Systems of Brantford, Ont., under the name iPET systems to supply complete preform molds with up to 192 drops. More details on iPET Systems were reported in October.