Multi-Tip Nozzles Get Individual Heat Control

Multi-tip hot-runner nozzles with individual temperature control on each nozzle tip are new from J-Tech Hot Runner Inc., Caledon, Ont.

Related Suppliers

Multi-tip hot-runner nozzles with individual temperature control on each nozzle tip are new from J-Tech Hot Runner Inc., Caledon, Ont. The nozzle comes with two to eight tips, depending on the material and part weight. The heaters, thermocouples, and nozzle tips are replaceable. Minimum tip distance is 10 mm with an overall bore diam. of 20 mm. For an eight-drop nozzle, overall bore diam. is 50 mm. Minimum nozzle length is 40 mm. Tel: (416) 619-0780 . www.jtechhotrunner.com

J-Tech Hot Runner Inc.
4314 Beech Grove Sideroad Caledon L7K 0M4, Ontario, Canada
Phone (519) 927-1067 Fax (519) 927-1068