WEB EXCLUSIVE: Novapol HB-W646-U is the latest HDPE from Nova Chemicals Corp., Pittsburgh, for large-part blow molding.
WEB EXCLUSIVE: Novapol HB-W646-U is the latest HDPE from Nova Chemicals Corp., Pittsburgh, for large-part blow molding. This UV-stabilized hexane copolymer (6.0 HLMI, 0.946 density) is aimed particularly at intermediate bulk containers (IBCs). It boasts excellent natural color for a more aesthetically pleasing container and outstanding flow and processability.
(800) 222-7213 • novachemicals.com