WEB EXCLUSIVE: A new grade of blow moldable PPS is used in a hot-water tank designed to withstand high temperatures in a line of European kitchen ovens from Miele & Cie. KG in Germany (U.S. office in Princeton, N.J.). Fortron MT9115L0 DW is a high-viscosity, 15% glass-filled grade said to be suited to blow molding complex geometries like this part. It can withstand continuous service temperatures up to 240 C/464 F and peaks up to 270 C/518 F and is approved for food contact. The blow molded tank supplies water for jets of steam that give bread a crispy crust and keep roasts tender inside while browning on the outside.