An improved version of a non-halogen flame-retardant concentrate for nylon reportedly offers a wider processing window than is usual for such products.
An improved version of a non-halogen flame-retardant concentrate for nylon reportedly offers a wider processing window than is usual for such products. PNM13319 FR concentrate from Techmer PM, Clinton, Tenn., was first introduced in 2006 for injection molding, but its newly enhanced versatility is said to extend its use to profi le extrusion. The product can enable nylons to meet UL 94V-0 and can be processed at up to 500 F. (865) 457-6700 • www.techmerpm.com