A new linear vibration welder from Forward Technology, Cokato, Minn., boasts a special servo-drive system that significantly raises performance of a small machine.
A new linear vibration welder from Forward Technology, Cokato, Minn., boasts a special servo-drive system that significantly raises performance of a small machine. Introduced at NPE this month, the new DLVW-2020 can handle upper tool weights up to 50 lb and a large weld area of 24 in.2 . The pneumatic machine is compact and meets cleanroom requirements. It can weld parts up to 20 x 20 in. and is housed in an "ultra-quiet" sound enclosure.
Forward Technology Industries
260 Jenks Ave. Cokato, MN 55321
Phone (320) 286-2578 Fax (320) 286-2467