Nylon 6 for Rotomolding

BASF Corp., Engineering Plastics, Wyandotte, Mich., is introducing its first nylon grade for rotomolding.

BASF Corp., Engineering Plastics, Wyandotte, Mich., is introducing its first nylon grade for rotomolding. Capron BR30HS nylon 6 is aimed at automotive liquid reservoirs. It is suitable for short runs of tanks for hydraulic oil, diesel fuel, or coolant reservoirs. Other potential uses are air-supply conduits and covers for trucks, construction machinery, forklifts, and tractors.