A new single-component pad-printing ink was developed specifically for adhesion to treated and untreated polypropylene, especially in medical applications. Fast-drying Polypro Ink 434 Series comes from ITW Trans Tech, Carol Stream, Ill. Other features include high gloss, fast drying, single component, and fast start-up, particularly in rotary systems. Initially, the ink series is available in black and white, but colors and high-density versions as well as medical Class VI grades are soon to be released. (630) 752-4000 • www.itwtranstech.com