The first medical-grade PC/ABS blends from Bayer MaterialScience, Pittsburgh, have been introduced for opaque parts such as surgical instruments, diagnostic devices, drug-delivery systems, and IV systems. Bayblend DP M850 and Bayblend DP M850XF meet the requirements of the FDA-modifi ed ISO 10933 Part 1 tests for biocompatibility. They can withstand sterilization by ethylene oxide, gamma radiation, and electronic-beam radiation. Easy-fl ow Bayblend DP M850XF is suited to thinwall components. Tel: (412) 777-2000 . www.bayerbms.com