WEB EXCLUSIVE: PEEK resin can penetrate more demanding wear applications, thanks to a new product from Victrex Polymer Solutions, West Conshohocken, Pa.
WEB EXCLUSIVE: PEEK resin can penetrate more demanding wear applications, thanks to a new product from Victrex Polymer Solutions, West Conshohocken, Pa. Victrex WG101 boasts lower wear rate and coefficient of friction than the workhorse wear-resistant grade, Victrex 450CF30. Unlike the latter, the new WG101 grade contains no PTFE. It has 30% higher compressive strength and almost 70% higher spiral flow at 1-mm thickness.