A new PET resin is designed to provide very high clarity and a wide processing window for molding thick-walled bottles and containers of unconventional sizes and shapes. Polyclear Crystal PET 3302 from Invista S.a.r.l Packaging resins, Charlotte, N.C., is said to offer outstanding moldability, fast cycles, and slow recrystallization. Besides a clear, high-gloss finish with plenty of sparkle, this resin reportedly provides exceptional strength and allows molding containers with tighter angles—even 90°. (877) 4INVISTA • www.polymers.INVISTA.com