A new polypropylene copolymer is said to provide the toughness and stiffness required for returnable containers, trays, nestable totes, and pallets.
A new polypropylene copolymer is said to provide the toughness and stiffness required for returnable containers, trays, nestable totes, and pallets. Marlex ALN-070 from Phillips Sumika Polypropylene Co., Houston, also boasts faster cycle times and reduced warpage, thanks in part to Milliken Chemical's Hyperform HPN-68L nucleating agent. Properties include a notched Izod impact of 1.0 ft lb/in. at -30 C, flexural modulus of 200,000 psi, and MFR of 7 g/10 min. (For more properties visit www.ptonline.com/mat_zone.)
Phillips Sumika Polypropylene
1301 McKinney St 13th Fl Houston, TX 77010
Phone (800) 392-2079 Fax (800) 994-9936