New NP114 prepreg of epoxy resin and DuPont's Nomex aramid paper is available from Norplex-Micarta, Postville, Iowa.

Related Suppliers

New NP114 prepreg of epoxy resin and DuPont's Nomex aramid paper is available from Norplex-Micarta, Postville, Iowa. NP114 reportedly offers superior electrical and thermal insulation for power-generation products and repairs. Insulation on through-bolts on electrical stators is a typical application. The prepreg also boasts fl ame-resistant properties. Thicknesses range from 3 to 15 mils. Tel: (563) 864-7321 . www.norplex-micarta.com