A new wear-resistant, MDI-based PUR elastomer formulation is designed for durable dunnage parts used for storage and transportation of delicate products, especially in automotive manufacturing.
A new wear-resistant, MDI-based PUR elastomer formulation is designed for durable dunnage parts used for storage and transportation of delicate products, especially in automotive manufacturing. Available from Chemline Inc., St. Louis, Chemthane 8010 offers Shore A hardness of 90 to 100, a 1:2 mix ratio by volume and a 6-min cure. Standard RIM equipment can be used. (314) 664-2230 • www.chemline. net
Chemline Inc.
5151 Natural Bridge Rd. St. Louis, MO 63115