Auger feeders for regrind and powder are now available on the two largest models of Guardian gravimetric batch blenders from Process Control Corp., Atlanta.
Auger feeders for regrind and powder are now available on the two largest models of Guardian gravimetric batch blenders from Process Control Corp., Atlanta. The company now offers its PF Series powder feeders as well as regrind feeders for 18-kg and 25-kg blender models, capable of up to 9600 lb/hr and blending up to 12 components. The auger feeders are already available on smaller sizes of 1.25 to 12 kg. (770) 449-8810 • www.processcontrol.com