Improved productivity and increased effi ciency are promised with the new release 8.0 of Moldfl ow Plastics Advisers (MPA) molding simulation software from Moldfl ow Corp. Framingham, Mass. MPA solids-based simulation software has been enhanced to help users analyze a broader range of parts with new 3D functionality. MPA 3D technology for thick, solid parts is based on Moldfl ow's high-end simulation product, Moldfl ow Plastics Insight (MPI). The Advanced 3D capability supplements MPA's patented Dual Domain analysis for thin-shell parts to increase the range of models that can be accurately analyzed by MPA. A new Optimal Technology Solution (OTS) automatically evaluates the model geometry to determine which analysis technology (Advanced 3D or Dual Domain) will achieve optimal results. Tel: (508) 358-584 . www.moldflow.com