TPE Solutions Inc., Shirley, Mass., is offering a new series of TPU alloys that are said to expand the hardness range available for overmolding and coextrusion.
TPE Solutions Inc., Shirley, Mass., is offering a new series of TPU alloys that are said to expand the hardness range available for overmolding and coextrusion. Up to now, most grades for these applications were typically 50 to 70 Shore A. The new Softlink 900 Series runs from 20 up to 90 Shore A. It is said to offer exceptional tensile and tear strengths relative to competing products of the same durometer. These off-white or easily colorable compounds do not require predrying.