The Select-Hesive line of liquid silicone rubbers for injection molding offer primerless adhesion when overmolded onto various thermoplastics.
The Select-Hesive line of liquid silicone rubbers for injection molding offer primerless adhesion when overmolded onto various thermoplastics. Supplied by Shincor Silicones, Inc., Akron, Ohio, sub. of Shin-Etsu Silicones of America, The Select-Hesive KE2090 series was introduced in 2007 with 30 to 70 Shore A hardness. It now also comes as soft as 10 to 20 Shore A. This series adheres to PC, PBT, and PPE/PPO compounds. (330) 630-9460 • www.shincor.com
Shincor Silicones
1030 Evans Ave Akron, OH 44305
Phone (330) 630-9460 Fax (330) 630-2857