A new type of TPV elastomers offers heat resistance up to 140 C for automotive and industrial applications such as window encapsulation, grommets and spouts for cable or hoses, air ducts, gaskets, and sealing profiles. Thermolast V compounds from Kraiburg TPE Corp., Duluth, Ga., are based on crosslinked SEPS in a PP matrix. Crosslinking of the modified PS end blocks reportedly provides superior long-term compression set at high temperatures. Available in hardnesses from 60 to 80 Shore A, the materials also offer good flow and strong adhesion to polyolefins. Tel: (678) 584-5020 . www.kraiburg-tpe.com
Kraiburg Corp
Ste 100
2625 N Berkley Lake Pkwy Duluth, GA 30096
Phone (678) 584-5020 Fax (678) 584-0500