A new double-indexable date stamper eliminates the need to mount two date stamps in a mold and to change one insert yearly.
A new double-indexable date stamper eliminates the need to mount two date stamps in a mold and to change one insert yearly. The new Multidater MD10 2006 from D-M-E Co., Madison Heights, Mich., has an engraved 12-month outer ring and a six-year inner ring (which are adjusted with a screwdriver) plus an arrow for the central insert. The surfaces are flush for all three rings. The date stamp is made from corrosion-resistant steel of 50 to 55 HRC that withstands temperatures up to 302 F.