The new CT (close-tolerance) line of ejector pins from D-M-E Co., Madison Heights, Mich., is designed for medical and electronic applications requiring critical tolerances. The pins have a 0.0002in. dimensional tolerance, while D-M-E’s standard pins hold a tolerance of 0.0003 in. The new pins are made from hardened M2 tool steel, which improves their ability to absorb defl ection without damage. Standard diameters are 0.0625 to 0.25 in. with no shoulder and up to 0.0937 in. with a 2-in. shoulder. Tel: (248) 398-6000 • www.dme.net