A new series of TPE alloys from GLS Corp., McHenry, Ill., were developed specifi cally for gaskets and seals.
A new series of TPE alloys from GLS Corp., McHenry, Ill., were developed specifi cally for gaskets and seals. Versafl ex CS5000 features low compression set (12% in 22 hr @ room temp.), comparable to TPVs at the same temperatures. Other properties include good melt stability, tensile and tear strength, and heat resistance. Injection and extrusion grades are available in hardnesses of 40 to 80 Shore A. Translucent pellets are easily colorable. No drying is required. Tel: (815) 385-8500 . www.glscorp.com
GLS Corporation
833 Ridgeview Drive McHenry, IL 60050
Phone (815) 385-8500 Fax (815) 385-8533