Two new unsaturated polyesters from Ashland Composite Polymers, Columbus, Ohio, are made with renewable resources.
Two new unsaturated polyesters from Ashland Composite Polymers, Columbus, Ohio, are made with renewable resources. Envirez 86400 INF for resin infusion and Envirez L 86300 for spray-up and hand lay-up contain 12% to 25% of Susterra bio-propanediol (bioPDO) from DuPont Tate & Lyle Bio Products Co. Bio-PDO is made by bacterial fermentation of corn sugar. (614) 790-4191 • www.ashspec.com