A new UV concentrate contains a proprietary additive said to eliminate the typical yellow hue of UV-stabilized PET.

Related Suppliers

A new UV concentrate contains a proprietary additive said to eliminate the typical yellow hue of UV-stabilized PET. Ampacet Corp., Tarrytown, N.Y., says its CrystalClear 603192-PT reduces yellowing because less than half as much additive is required. What’s more, the new product reportedly offers the same level of UV protection at up to 40% lower cost. (914) 631-6600 • www.ampacet.com