MoldWiz 985JB is a new concentrated water-based mold release for SMC/BMC molding. This proprietary formulation from Axel Plastics Laboratories, Inc., Woodside, N.Y., is an easy-wetting, quickdrying, 36%-active solution. It can be diluted to 5%-active with plain tap water and reportedly will remain fully emulsified without constant agitation. This release is said to yield clean parts that are ready for secondary operations. The product’s neutral pH and quick-drying nature is said to make it non-corrosive and suitable for use on steel, aluminum, and most other mold substrates. It is applied with a hand-pumped spray bottle to “fog” the mold with a light mist and/or a quick wipe across the mold with a cotton rag. Typically, the release is applied every three to five parts. This product reportedly is much less prone to buildup than many other releases, but any excess can easily be removed with warm water. (718) 672-8300 • www.axelplastics.com