Three new high-melt-index TiO2 masterbatches originally engineered for injection molding of thin-wall PE containers have been adapted for film extrusion and blow molding.
Three new high-melt-index TiO2 masterbatches originally engineered for injection molding of thin-wall PE containers have been adapted for film extrusion and blow molding. Developed by Techmer PM, they are suitable for food contact under sections 170-199 of CFR 21 and boast compatibility with most PE resins, including LDPE, LLDPE, mLLDPE, HDPE, and EVA. They can be processed at up to 600 F. PM13215E41 is a 125-MI grade, while PM13214E4 and PM13213E16 have MIs of 85 and 50, respectively. They will be featured at NPE in June.
Techmer PM, LLC
1 Quality Circle Clinton, TN 37716
Phone (865) 457-6700 Fax (865) 457-3012