EXTRUSION: Why Bother to Chrome Plate Your Screws?
It doesn’t add that much to the overall cost and can improve performance and facilitate maintenance. So the better question is: Why not?
Chrome plating adds only about 10% to the cost of a typical screw and it provides so many benefits with almost no performance disadvantages. Yet many processors opt not to go with such screws.
There are two basic kinds of chrome plating. That which is used on an automobile bumper, for example, is called decorative plating and is relatively soft. The kind used for screws is called hard chrome or industrial chrome. Hard chrome has a hardness of 65-69 Rc, which is equal to the hardest tool steels.
For screw plating, the coating is typically about 0.001 in. thick and does not materially affect the geometry of even the most critical dimensions. Additionally, it has a bond strength of approximately 6000 psi when properly applied, so it almost never comes off due to abrasion. That said, chrome plating is not suitable for the tops of the screw flights, where the stress can easily exceed 6000 psi. During the plating process, screw flights are almost always masked off.
Chrome plating provides a good corrosion barrier to everything but some acids formed by the degradation of certain polymers. Acids do not actually affect the chrome, but hard chrome inherently has micro cracks. Acids can seep through the cracks and get under the chrome layer to corrode the bond. These cracks are impossible to see with the naked eye but are readily visible under magnification.
Most of the time this risk can be addressed by applying chrome in several thin layers so the cracks do not intersect, thereby providing a largely impervious surface. That treatment is often used on rigid PVC processing equipment and is referred to as double or even triple chrome. It requires a series of separate plating treatments and cannot be duplicated by simply applying a thicker coating.
The simplest and most common reason to chrome plate screws is that they do not rust while in storage or during shipping. To prevent rusting during those periods, it’s necessary to coat non-chromed screws with a temporary protective coating, which is messy to put on and even messier to take off.
The inherent smoothness and lubricity of polished hard chrome makes it much easier to clean screws, either manually or by purging. Hard chrome can be polished to <0.5 Ra, which is a true mirror finish, and in that form has a coefficient of friction (COF) less than one-quarter of that of polished steel. During periodic cleaning, it’s common to use wire brushes and various scrapers.
Hard chrome resists abrasion from these tools, which often roughen the surface of uncoated steel, making for shorter and shorter cleaning intervals. Additionally, the inherent lubricity of chrome reduces its bond to the polymer, making it easier to remove.
Hard chrome is effective in preventing abrasive wear from many of the fillers used in polymers. Because of the combination of high hardness, low COF, and good lubricity, low loadings of even very hard materials like calcium carbonate or titanium dioxide will not readily damage hard-chrome plating.
However, as loading percentages increase or even harder fillers are added, a somewhat more aggressive wear mechanism develops, requiring more sophisticated and expensive surface-protection coatings. But ordinarily the low COF and lubricity of polished chrome can improve the extruder’s feed rate, which governs the output of the screw in many cases.
The principle of solids feeding for a given polymer characteristic and mechanical arrangement is that the transport of the polymer is proportional to the difference between the drag of the solid polymer particles on the barrel and their drag on the screw channel. By reducing the frictional drag in the screw channel, the feed rate can be increased and made more consistent.
Additionally, the higher lubricity of chrome plating reduces the tendency of polymer to stick to the screw in the solids feeding area (resulting in so-called “collars”). Chrome plating has been known to eliminate the need for screw cooling with polymers that have a tendency to stick to the screw in the solids area when it is hot and not rotating.
Simply put, hard-chrome plating is a very cost-effective solution to a lot of problems encountered during the life of the screw.
Related Content
Improve Production Rates Via Screw Design — Barrier vs. General Purpose vs. Melt Uniformity
I’m looking for a few good molders to help trial a new screw design, and share data and results for a future article to prove the benefits of a melt uniformity screw.
Read MoreImprove Quality & Productivity With Advanced Screw Design
Most molders are still running with screw designs that haven’t changed much in 30 years. But they don’t need to.
Read MoreHow Screw Design Can Boost Output of Single-Screw Extruders
Optimizing screw design for a lower discharge temperature has been shown to significantly increase output rate.
Read MoreXaloy Invests in New R&D Center
Xaloy is investing in a new R&D Facility for plasticizing equipment in northeast Ohio with aid from JobsOhio R&D Center Grant.
Read MoreRead Next
Understanding Melting in Single-Screw Extruders
You can better visualize the melting process by “flipping” the observation point so that the barrel appears to be turning clockwise around a stationary screw.
Read MoreHow Polymer Melts in Single-Screw Extruders
Understanding how polymer melts in a single-screw extruder could help you optimize your screw design to eliminate defect-causing solid polymer fragments.
Read MorePeople 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems
Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.
Read More