Gravimetric Feeding Systems For Molding and Extrusion
A continuous loss-in-weight feeding system and a gravimetric additive feeder are new from ACS Group, New Berlin, Wis.
New Product Announcements Published: 8/1/2009
Continuous Gravimetric Blender Feeds Multiple Powders
Process Control Corp., Atlanta, has brought out its first continuous gravimetric powder blender.
New Product Announcements Published: 7/1/2009
Gravimetric Blender Boasts Added Precision
Whereas most batch gravimetric blenders weigh each ingredient one at a time into a blender bowl, Plast Control’s first gravimetric blender has two weigh chambers with load cells.
New Product Announcements Published: 6/1/2009
Gravimetric Dispensing Of a Single Ingredient
AccuDispense is a new single-ingredient gravimetric dispensing unit from Process Control Corp., Atlanta.
New Product Announcements Published: 4/1/2009
‘Quick Ship’ Blenders and Lower Prices For Gravimetric Extrusion Control
WEB EXCLUSIVE Process Control Corp., Atlanta, has a new Quick Ship program for three of its most popular sizes of Guardian batch weight blenders.
New Product Announcements Published: 4/1/2009
Low-Rate Feeder Has Disposable EPDM Hopper
New PureFeed AI-300 feeder from Schenck AccuRate, Whitewater, Wis., is designed for metering additives at rates as low as 1.1 lb/hr, though larger feed augers are available for up to 330 lb/hr.
New Product Announcements Published: 3/11/2009
New Loader Enhances Weigh Feeding
A new approach to loading a hopper-mounted gravimetric feeder is said to improve accuracy so molders and extruders can save on colors and additives.
New Product Announcements Published: 3/1/2008
Feeders Go Wireless
Volumetric and gravimetric feeders from Schenck AccuRate, Whitewater, Wis., now can have optional Bluetooth wireless technology.
New Product Announcements Published: 3/1/2008
Vibratory Feeder for Precise Gravimetric Metering
A new vibratory gravimetric metering feeder was introduced at the recent K 2007 show by Brabender Technologie (North American office in Mississauga, Ont.). Its DualTray Feeder consists of two or more cylindrical feed modules, each with a semicircula...
New Product Announcements Published: 2/1/2008
Larger Weigh Blender For Extrusion
A larger model with 18 kg (40 lb) capacity has been added to the Guardian of batch gravimetric blenders from Process Control Corp., Atlanta.