This past spring, Dutch brewer Heineken introduced a colored 4-liter PET keg for its Amstel brand of beer in the Benelux region of Europe. ArticlePublished: 8/23/2011
Last month, PepsiCo Beverages Canada, Mississauga, Ont., unveiled what’s said to be North America’s first soft-drink bottle made from 100% recycled PET. ArticlePublished: 7/27/2011
Many manufacturing sites operate on the assumption that compressed air is free. Usage is totally uncontrolled, and open air lines cost real money. ArticlePublished: 6/27/2011
WEB EXCLUSIVE: In a somewhat unusual move, two major consumer brands will cosponsor next month’s BioPlastek 2011 Forum on Bioplastics in N.Y.C. ArticlePublished: 4/29/2011
WEB EXCLUSIVE: PepsiCo, Purchase, N.Y., says it has developed the world’s first PET bottle made entirely from plant-based, renewable resources. ArticlePublished: 4/29/2011