Last month we briefly discussed the influence of temperature on the mechanical properties of polymers and reviewed some of the structural considerations that govern these effects. ColumnsPublished: 8/23/2011
The polymers we work with follow the same principles as the body: the hotter the environment becomes, the less performance we can expect. ColumnsPublished: 7/27/2011
When you’re already a leader in your industry, you might be tempted to simply stay the course and not worry about issues such as sustainability and carbon footprint. ColumnsPublished: 1/4/2011
Prices of commodity resins other than PVC moved up in September—and, in the case of polypropylene, rose a bit more in October. ColumnsPublished: 1/4/2011
Lower prices for all four major commodity thermoplastics were the trend from late April to mid-May, with good potential for further downward movement this month and beyond ColumnsPublished: 6/1/2010