Mixing and extruding wood fiber in a plastic matrix is technically demanding. It requires careful attention to formulation, drying, and extrusion temperatures ArticlePublished: 4/26/2012
Some 18 months in the making, Polymera Inc. last month announced that its 160,000 ft² production plant is officially open for business, with annual capacity for 60 million lb of wood/plastics composite (WPC) compounds. ArticlePublished: 1/27/2012
Polywood Inc. in Edison, N.J., uses mixed recycled plastics to make fiber-reinforced structural profiles for railroad ties, I-beams, and decks. ArticlePublished: 6/7/2010
Three years ago, when Martin Grohman and Michael Hurkes started Correct Building Products in Biddeford, Me., it wasn’t so much a start-up as a rocket launch. ArticlePublished: 6/1/2010
In December, about a dozen representatives of European chemical companies gathered in Aachen, Germany, to celebrate the 20th anniversary of a quiet revolution in plastics. ArticlePublished: 2/1/2009
WEB EXCLUSIVE A new organic biocide is said to significantly increase the lifespan of wood plastic composites (WPCs), by ‘dramatically’ reducing the adverse effects of mold or microorganisms that cause discoloration. ArticlePublished: 12/17/2008