PUBLISHED: 9/23/2014

AUXILIARIES: News in Drying, Blending, Cooling, Granulating at Fakuma Show

Wittmann Battenfeld to display wide array of new auxiliaries at show.


PUBLISHED: 9/9/2014

MATERIALS HANDLING: Bulk Container Dumper For High-Bulk-Density Materials

Unit is made of specially milled 304-2b stainless-steel sheet that is said to have a greatly reduced coefficient of friction compared with typical flat sheet.


PUBLISHED: 7/29/2014

AUXILIARY EQUIPMENT: Tapered BFM Fitting Offers Surge Bin Visibility

Facilitates clean out of powdered materials as well.


PUBLISHED: 6/17/2014

AUXILIARIES: Low-Dose Blender for Small Machines

Gravimetric blender feeds up to 572 lb/hr in doses down to 3 g per component.


PUBLISHED: 4/25/2014

AUXILIARIES: Low-Dose Blender for Small Machines

It meters down to 3 g per component.


PUBLISHED: 10/24/2013

AUXILIARIES: ‘User-Friendly’ Batch Blender Now Has More Capacity

Process Control debuts larger, 2-kg version of its Guardian Series 3 batch blender.


PUBLISHED: 9/24/2013

AUXILIARIES: Small-Frame Continuous Blender

The X2D6 is a new continuous blender from Process Control Corp. that handles throughputs up to 660 lb/hr.


PUBLISHED: 8/28/2013

AUXILIARIES: New & Upgraded Blenders at K 2013

New gravimetric blenders from Motan-Colortronic, Koch-Technik, and ProTec, plus an upgrade from Wittmann.


PUBLISHED: 5/28/2013

AUXILIARIES: Easy-Cleaning Blender And Beefed-Up Mold TCU

At its Competence Days open house in Austria in April, Wittmann Battenfeld GmbH (U.S. office in Torrington, Conn.) unveiled two new auxiliaries for plastics processing.


PUBLISHED: 12/28/2012

AUXILIARIES: Blenders Handle Difficult Scrap

Two new solutions from Conair, Cranberry Township, Pa., are designed for use with its TrueBlend line of blenders to allow feeding thin, flaky regrind without repelletizing.