Additive Manufacturing

Exploring the: Additive Manufacturing Zone

32 Results for: New Product

Sort by:
Published: 8/24/2018

Materials: First 3D Printing Flexible Material Based on PEBA
3D printed parts made from Evonik’s PEBA powder boast high flexibility, resistance to chemicals and outstanding durability.  

Published: 7/23/2018

Additive Manufacturing: First High-Purity PVDF 3D Printing Filament
Based on Arkema’s Kynar PVDF, Nile Polymer’s new filament is designed for large parts without dimensional warping.

Published: 7/13/2018

Additive Manufacturing: Production-Ready Materials For 3D Printing
One is an elastomeric PUR.

Published: 5/9/2018

3D Printing for Production Takes Hold at Forecast 3D
The company is seeing real benefits and potential in HP’s Multi Jet Fusion (MJF) 3D printing technology for manufacturing plastic parts in high volumes.

Published: 3/26/2018

Arburg Molding Cells Show Off LSR, High-Speed Packaging, Automotive Composites, and Industry 4.0
Arburg’s nine exhibits include an Allrounder 1120H (730 U.S. tons), molding eight components of folding step stool from a family mold and assembling via robot.

Published: 3/15/2018

Conformal Cooling Product Lines for Injection Molding and Blow Molding
Conformal cooling is a design approach for improving mold and die productivity that can save 10-50 percent or more on cycle time, in addition to quality benefits and improved tooling durability.

Published: 2/23/2018

Gamut of New Technologies for Compounding
Leistritz Extrusion’s wide-ranging display of twin-screw extruder related technologies at NPE2018 includes a system for manufacturing 3D filaments.   

Published: 2/18/2018

Additive Manufacturing: HP Announces Lower-Cost Jet Fusion 3D Printers for Prototyping—in Full Color
Lower cost, more compact models for low-volume prototyping also introduce full-color 3D printing.

Published: 2/18/2018

Injection Molding: At NPE, U.S. Debut of Arburg’s Largest Machine Yet in a Brand-New Design
Besides a brand-new machine design, Arburg will present cells molding automotive composites, medical, LSR, and packaging applications, as well as Industry 4.0 multiprocess integration and Freeformer 3D printing.

Published: 2/18/2018

Tooling: Metal 3D Printer and High-Speed Milling in One Machine
Laser sinter metal powder and perform CNC machining of tooling components in the same machine.