AGY Buys Glass Mat Plant from OC

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Glass-fiber producer AGY, Aiken, S.C., has agreed to buy the continuous-filament mat (CFM) business and plant in Huntingdon, Pa., from Owens Corning, Toledo.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Related Suppliers

Glass-fiber producer AGY, Aiken, S.C., has agreed to buy the continuous-filament mat (CFM) business and plant in Huntingdon, Pa., from Owens Corning, Toledo. CFM will be a new business for AGY.