AGY Expands S-2 Glass Capacity 50%

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

AGY, Aiken, S.C., has raised its capacity for S-2 glass reinforcements by 50% and can add more capacity quickly when required.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Related Suppliers

AGY, Aiken, S.C., has raised its capacity for S-2 glass reinforcements by 50% and can add more capacity quickly when required. Extra capacity was needed to armor military vehicles for use in Iraq and Afghanistan.