Asahi Glass to Expand ETFE

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Asahi Glass Co. (AGC) of Japan will expand capacity for Fluon ETFE fluoropolymer by 20% in the U.K. by next January.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon
Asahi Glass Co. (AGC) of Japan will expand capacity for Fluon ETFE fluoropolymer by 20% in the U.K. by next January. It will strengthen AGC’s position as the world’s leading producer of ETFE. AGC says this expansion is needed to meet demand in the U.S. and Europe for wire and cable, automotive, construction, and film uses. AGC Chemicals Americas, Inc. is in Bayonne, N.J.