New Name in Auto Glazing

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Bayer MaterialScience AG (U.S. office in Pittsburgh), which recently sold its share of the Exatec joint venture to partner SABIC Innovative Products (formerly GE Plastics), has created a new umbrella brand for its auto-glazing activities.

Related Suppliers

Bayer MaterialScience AG (U.S. office in Pittsburgh), which recently sold its share of the Exatec joint venture to partner SABIC Innovative Products (formerly GE Plastics), has created a new umbrella brand for its auto-glazing activities. BayVision is the name representing its full range of expertise in glazing materials and know-how in molding, engineering development, and coatings. The first vehicle to bear the BayVision logo is the i-mode concept car (photo), developed with Hyundai and unveiled at the 2008 Geneva Auto Show. It has 11 glazing components of Bayer’s Makrolon polycarbonate. (800) 662-2927 • www.bayermaterialsciencenafta.com

Resources